thenounproject_com_20180725_153659.jpg

Anode & Cathode Ink

Cathode Ink

Descriptions

  • There is no need for any specific or expensive post treatment process to activate their properties.

  • It can therefore be processed on aluminium substrate by various techniques:Doctor blade printing, Screen-printing

  • ​It is easily solubilized in various solvents, showing unique properties such as:

01

Low cost solution

03

Tight quality control to ensure reproducibility

02

Low material and processing cost

04

Custom formulation for each printing need.

Instructions

      For a 13 100 μm thickness film by doctor blade printing:

  • Place the ink in ultrasonic bath around 60 minutes.

  • Then place it in a mechanical stirring between 30 60 minutes. The ink is ready to be used.

  • After the printing process, the ink should be cured at 80 °C during 60 minutes.

Specification

MAGRON CO., LTD

 (15588) #403 3dong, Gyeonggi Technopark, 705 Haean-ro, Sangnok-gu, Ansan-Si, Gyeonggi-do, Republic of Korea

copyright ⓒ 2014 MAGRON

All Rights Reserved.

TEL : 82-31-500-4633, 82-31-400-3757

FAX : 82-31-500-4631

  • Grey Facebook Icon
  • Grey YouTube Icon